  • 锡单晶 50Sn118.69


    说明:锡是柔软的,柔韧的银白色金属。表面有氧化膜时不与氧气和水反应。锡溶于酸和碱。被用于焊料合金,锡板,聚合物添加剂和一些防污涂料。


    锡单晶性能参数


    状态:

    单晶


    晶体结构:

    tetragonal


    生产方法:

    Bridgeman


    标准尺寸:

    diameter 9-10mm

    thickness 1-2mm


    晶向:

    (100), (110) and (111)


    晶向精度:

    <2°, <1°, <0.5° or <0.1°


    纯度:

    as cut, one or two sides polished


    表面粗糙度:

    <0.03μm


    典型分析:

    99.999%


    典型分析(ppm):

    C 6

    H < 1

    O < 5

    N < 5

    Bi 0.5

    Cl 0.4

    Co < 1

    Fe 0.25

    Mg 0.15

    Ni < 0.3

    P 1

    Pb 1.5

    S 0.6

    Si 0.3

    Ta < 1

    Ti 0.15

    W 0.2

    Sn balance


    其他性能参数


    晶体结构:

    (cell dimensions/pm), space group

    a-Sn (grey) cubic (a=648.92), Fd3m

    b-Sn (white) tetragonal (a=583.16,

    c=318.13), I42/amd

    T(a->b)=286.4 K [b form at room temperature]

    X射线衍射质量吸收系数:

    CuKa 256 (μ/r) / cm2g-1 MoKa 31.1 (μ/r) / cm2g-1

    中子散射距离:

    0.6225 b/10-12 cm

    热中子捕获横截面:

    0.626 sa / barns

    密度:

    7.30 g/cm3

    熔点:

    231.968 °C / 505.118 °K

    沸点:

    2269.85 °C / 2543 °K

    摩尔体积:

    16.24 (b) cm3

    导热系数:

    66.6 (a) [300 K] Wm-1K-1

    热膨胀线系数:

    5.3 x 10-6 (a) K-1

    21.2 x 10-6 (b) K-1

    电阻系数:

    11.0x10-8 (a) [273 K] Wm

    聚磁敏感性:

    -4.0 x 10-9(a) kg-1m3

    +3.3 x 10-10(b) kg-1m3

    杨氏模量:

    49.9 GPa

    刚性模量:

    18.4 GPa

    体积模量:

    58.2 GPa

    泊松比:

    0.357 GPa

    半径:

    Sn4+ 74; Sn2+ 93; Sn4- 294; atomic 141; covalent 140; van der Waals 200

    负电性:

    1.96 (Pauling); 1.72 (Allred); 4.30 eV (absolute)

    有效核电荷:

    5.65 (Slater); 9.10 (Clementi); 11.11 (Froese-Fischer)

    同位素:

    37

    同位素质量范围:

    106 -> 132


    生物资料


    生物类别:

    May be essential to some organisms, including human.

    毒性


    毒性摄取量:

    low toxicity as metal and some inorganic tin (II) salts

    致命摄取量:

    LD50 (SnCl2, oral, rat) = 700 mg kg-1

    危险性:

    Tin (II) salts can be pisonous by ingestion and other routes and there is evidence that tin can have experimental carcinogenic and human mutagenic effects. Some organotin compounds are very toxic.

    人体等级


    血液:

    c. 0.38 mg dm-3

    骨骼:

    1.4 p.p.m.

    肝脏:

    0.23 - 2.3 p.p.m.

    肌肉:

    0.33 - 2.4 p.p.m.

    每日食物摄取量:

    0.2 - 3.5 mg

    70kg成人平均总元素含量:

    20 mg


    地质资料


    矿物:

    Many minerals are known, and aluminium is present in many other minerals

    矿物化学式

    公式

    密度

    硬度

    晶体外观

    Cassiterite

    SnO2

    6.99

    6 - 7

    tet., adam./ met. brown


    主要矿石:

    cassiterite

    世界产量:

    165 000 tonnes/year

    主要矿区:

    Malaysia, Sumatra, Russia, China, Bolivia, Zaire

    储量:

    4.5 x 106 tonnes

    样品:

    available as bars, breads, foil, granules, rod, shot and wire. Safe.


    总含量


    太阳:

    100 (relative to H = 1 x 1012)

    地壳:

    2.2 p.p.m.

    海水:


    大西洋表面:

    2.3 x 10-6 p.p.m.

    大西洋深处:

    5.8 x 10-6 p.p.m.

    停留时间:

    n.a.

    类别:

    scavenged

    氧化态:

    IV

地址:北京市昌平区霍营街道紫金新干线四区3号楼2层207室

电话:010-82867922

传真:010-82867919

邮箱:contact@germantech.com.cn

关注我们

扫一扫

您有什么问题或要求吗? 点击下面,我们很乐意提供帮助。 联系我们
Copyright © 2022 北京汇德信纳米科技有限公司    京ICP备2023001877号-1